The use of PP fillers has
a phenomenon of poor plasticization, which has many constraints on the
development of PP fillers. In order to solve this problem, the continuous
research of PP filler manufacturers showed that it is likely to be the quality
of fillers that caused poor dispersion.
There are currently five
common methods for changing this problem. Increase the injection temperature of
PP, and increase the decomposition temperature of PP at a safe temperature of
about 300 degrees to increase the back pressure. The filler masterbatch with lower
mesh should be used, the mesh may be the cause of uneven packing dispersion. A
relatively low mesh has better dispersion. Add some lubricating dispersant and
improve the production process. If the requirements for filler masterbatch are
relatively high, it is recommended to use the transparent filler masterbatch on
the market, the effect will be better.
The problems caused by PP
fillers require further research until the problem can be solved very
effectively. The development of PP fillers requires strong technology as
support, and problems are solved in a timely manner, so as to promote the
continuous advancement of PP fillers.